Bars

Bars:

Fusible Alloys, High Purity Indium Bars, Indium Alloy Bars, Pure Indium Bars, Pure Metal Bars (Non Indium), Wave Solder Bars

  • Purchase this item

    117°F Eutectic117°F Eutectic

    IPN: Ingotbn-05117-5lbIG

    Price: $750.00

    Typical Properties:
    #117 Alloy

    Eutectic Alloy

    Liquidus: 117F - 47C
    Solidus: 117F - 47C

    Yield Temperature: 117F
    Weight: 0.32 lb/in3
    Tensile strength: 5.4 ksi
    Slow-load elongation: 1.5%
    Brinell hardness: 12

    Specific Heat
    Liquid: 0.035 Btu/lb-F
    Solid: 0.035 Btu/lb-F
    Latent heat of fusion: 6Btu/lb
    Coefficient of thermal expansion: 14
    Electrical conductivity: 3.9% Cu

    Fusible Alloys include a group of binary, ternary, quaternary, and quinary alloys containing Bismuth, lead, tin, cadmium and indium. The term fusible alloy refers to any of the more than 100 white-metal alloys that melt at relatively low temperatures.

    Fusible alloys are materials that melt at less than 300F, well below the melting point of Tin-lead eutectic solders. The major component of fusible alloys is bismuth. Besides producing low melting point, bismuth also gives these materials the unique characteristic of expanding on freezing. This expansion, which can continue for hours or even days after freezing, has proven to be a useful property in many processes.

    Fusible Alloys are classified as either eutectic or non-eutectic. In eutectic alloys, the melting point coincides with the freezing point. Non- eutectic alloys exhibit a range between the melting and freezing point in which the material is "mushy" or "pasty".

    Fusible Alloys are used for lens blocking and tube bending, for anchoring chicks and fixtures and for mounting thin sections such as gas turbine blades for machining. The eutectic fusible alloys, which can be tailored to give s specific melting point, find applications in temperature control devices and in fire protection devices. Details…

  • Purchase this item

    136°F Eutectic136°F Eutectic

    IPN: Ingotbn-05136-2.5lbIG

    Price: $545.00

    Typical Properties:
    #136 Alloy

    Eutectic Alloy

    Liquidus: 136F - 58C
    Solidus: 136F - 58C

    Yield Temperature: 136F
    Weight: 0.31 lb/in3
    Tensile strength: 6.3 ksi
    Slow-load elongation: 50%
    Brinell hardness: 14

    Specific Heat
    Liquid: 0.032 Btu/lb-F
    Solid: 0.032 Btu/lb-F
    Latent heat of fusion: 8Btu/lb
    Coefficient of thermal expansion: 13
    Electrical conductivity: 3.0% Cu

    Fusible Alloys include a group of binary, ternary, quaternary, and quinary alloys containing Bismuth, lead, tin, cadmium and indium. The term fusible alloy refers to any of the more than 100 white-metal alloys that melt at relatively low temperatures.

    Fusible alloys are materials that melt at less than 300F, well below the melting point of Tin-lead eutectic solders. The major component of fusible alloys is bismuth. Besides producing low melting point, bismuth also gives these materials the unique characteristic of expanding on freezing. This expansion, which can continue for hours or even days after freezing, has proven to be a useful property in many processes.

    Fusible Alloys are classified as either eutectic or non-eutectic. In eutectic alloys, the melting point coincides with the freezing point. Non- eutectic alloys exhibit a range between the melting and freezing point in which the material is "mushy" or "pasty".

    Fusible Alloys are used for lens blocking and tube bending, for anchoring chicks and fixtures and for mounting thin sections such as gas turbine blades for machining. The eutectic fusible alloys, which can be tailored to give s specific melting point, find applications in temperature control devices and in fire protection devices. Details…

  • Purchase this item

    158°F Eutectic158°F Eutectic

    IPN: Ingotbo-05158-3.75lbIG

    Price: $262.50

    Typical Properties:
    #158 Alloy

    Eutectic Alloy

    Liquidus: 158F - 70C
    Solidus: 158F - 70C

    Yield Temperature: 158F
    Weight: 0.339 lb/in3
    Tensile strength: 5.99 ksi
    Slow-load elongation: 200%
    Brinell hardness: 9.2

    Specific Heat
    Liquid: 0.040 Btu/lb-F
    Solid: 0.040 Btu/lb-F
    Latent heat of fusion: 14Btu/lb
    Coefficient of thermal expansion: 12
    Electrical conductivity: 4.0% Cu

    Fusible Alloys include a group of binary, ternary, quaternary, and quinary alloys containing Bismuth, lead, tin, cadmium and indium. The term fusible alloy refers to any of the more than 100 white-metal alloys that melt at relatively low temperatures.

    Fusible alloys are materials that melt at less than 300F, well below the melting point of Tin-lead eutectic solders. The major component of fusible alloys is bismuth. Besides producing low melting point, bismuth also gives these materials the unique characteristic of expanding on freezing. This expansion, which can continue for hours or even days after freezing, has proven to be a useful property in many processes.

    Fusible Alloys are classified as either eutectic or non-eutectic. In eutectic alloys, the melting point coincides with the freezing point. Non- eutectic alloys exhibit a range between the melting and freezing point in which the material is "mushy" or "pasty".

    Fusible Alloys are used for lens blocking and tube bending, for anchoring chicks and fixtures and for mounting thin sections such as gas turbine blades for machining. The eutectic fusible alloys, which can be tailored to give s specific melting point, find applications in temperature control devices and in fire protection devices. Details…

  • Purchase this item

    1kg 99.9% In Ingot1kg 99.9% In Ingot

    IPN: Ingotic-05376-1kIG

    Price: $792.50

    Typical Indium Analysis
    99.9%


    PPMWT
    Fe : 10-20
    Ni : 5-20
    Cu : 5-30
    Cd : 50-100
    Pb : 200-300
    Sn : 50-200
    Ti : 100-300

    Analysis by OES

    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details…

  • Purchase this item

    1kg 99.99% In Ingot1kg 99.99% In Ingot

    IPN: Ingotic-05373-1kIG

    Price: $810.00

    Typical Indium Analysis
    99.99%


    PPMWT
    Fe : 1-2
    Ni : 2-6
    Cu : 2-6
    Cd : 5-10
    Pb : 10-30
    Sn : 10-25
    Ti : 1-4

    Analysis by OES

    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details…

  • Purchase this item

    1kg 99.999% In Ingot1kg 99.999% In Ingot

    IPN: Ingoti5-05374-1kIG

    Price: $845.00

    Typical Indium Analysis
    99.999%


    PPMWT
    Fe : 0.5
    Ni : 1.0
    Cu : 1.0
    Cd : 1.0
    Pb : 2.0
    Sn : 2.5
    Ti : 1.0

    Analysis by OES

    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details…

  • Purchase this item

    1lb 90In 10Sn Alloy Bar1lb 90In 10Sn Alloy Bar

    IPN: Ingotia-05538-1lbIG

    Price: $489.09

    Indium-tin alloys are useful where lower temperatures are required to protect heat-sensitive components and substrates. The indium-tin eutectic with a sharp melting point has excellent wettability on nonmetallic materials. It also has good low-temperature malleability and compensates for some difference in the coefficients of thermal expansion of dissimilar metals. The addition of either metal to the other increases the corrosion resistance of the resulting alloy.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details…

  • Purchase this item

    1lb 91In 9Sn Alloy Bar1lb 91In 9Sn Alloy Bar

    IPN: Ingotia-05887-1lbIG

    Price: $360.23

    Indium-tin alloys are useful where lower temperatures are required to protect heat-sensitive components and substrates. The indium-tin eutectic with a sharp melting point has excellent wettability on nonmetallic materials. It also has good low-temperature malleability and compensates for some difference in the coefficients of thermal expansion of dissimilar metals. The addition of either metal to the other increases the corrosion resistance of the resulting alloy.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details…

  • Purchase this item

    500g 99.9% In Ingot500g 99.9% In Ingot

    IPN: Ingotic-05376-500gIG

    Price: $0.87

    Typical Indium Analysis
    99.9%


    PPMWT
    Fe : 10-20
    Ni : 5-20
    Cu : 5-30
    Cd : 50-100
    Pb : 200-300
    Sn : 50-200
    Ti : 100-300

    Analysis by OES

    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details…

  • Purchase this item

    500g 99.99% In Ingot500g 99.99% In Ingot

    IPN: Ingotic-05373-500gIG

    Price: $0.88

    Typical Analysis

    99.99% Indium

    PPMWT
    Fe : 1-2
    Ni : 2-6
    Cu : 2-6
    Cd : 5-10
    Pb : 10-30
    Sn : 10-25
    Ti : 1-4

    Analysis by OES


    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details…

  • Purchase this item

    500g 99.999% In Ingot500g 99.999% In Ingot

    IPN: Ingoti5-05374-500gIG

    Price: $0.92

    Typical Indium Analysis
    99.999%


    PPMWT
    Fe : 0.5
    Ni : 1.0
    Cu : 1.0
    Cd : 1.0
    Pb : 2.0
    Sn : 2.5
    Ti : 1.0

    Analysis by OES

    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details…

  • Purchase this item

    Indium Bar 6n min 1kgIndium Bar 6n min 1kg

    IPN: Ingoti6-05375-1kIG

    Price: $1310.00

    We produce 6N material with impurities held to less than 100 ppb/weight as analyzed by OES. 6N (and often 5N) indium is selected when the user's application offers enough flexibility to allow the balancing of device performance with material cost. Details…

  • Purchase this item

    Indium Bar 6n min 500gIndium Bar 6n min 500g

    IPN: Ingoti6-05375-500gIG

    Price: $1.92

    We produce 6N material with impurities held to less than 100 ppb/weight as analyzed by OES. 6N (and often 5N) indium is selected when the user's application offers enough flexibility to allow the balancing of device performance with material cost. Details…

  • Purchase this item

    Indium Bar 6n5 min 1kgIndium Bar 6n5 min 1kg

    IPN: Ingoti6-05816-1kIG

    Price: $1410.00

    This purity is especially suited for the production of single crystal III-V compound semiconductors, such as indium Phosphide used as substrates for fabrication of integrated circuits or discrete devices such as laser diodes and photo detectors. Certification of 6N5 purity is by OES (optical emission spectroscopy) with GFAA (graphite furnace atomic absorption) being used for quantitative analysis of selected elements. Details…

  • Purchase this item

    Indium Bar 6n5 min 500gIndium Bar 6n5 min 500g

    IPN: Ingoti6-05816-500gIG

    Price: $2.01

    This purity is especially suited for the production of single crystal III-V compound semiconductors, such as indium Phosphide used as substrates for fabrication of integrated circuits or discrete devices such as laser diodes and photo detectors. Certification of 6N5 purity is by OES (optical emission spectroscopy) with GFAA (graphite furnace atomic absorption) being used for quantitative analysis of selected elements. Details…

  • Purchase this item

    Indium Bar 6n5 WCI 1kgIndium Bar 6n5 WCI 1kg

    IPN: Ingoti6-05989-1kIG

    Price: $1860.00

    Our 6N5WCI (with controlled impurities) indium is refined for use in critical bulk crystal growth and in epitazial processes including molecular beam (MBE), liquid phase (LPE), and vapor phase (VPE) epitazy 6N5WCI is tailored for applications requiring the stringent control of impurities which, until now, only a 7N purity level may have provided at higher cost. This is accomplished by holding total metallic impurities to less than 500 ppb/weight (by GDMS), with particular attention given to maintaining low levels of elements known to be detrimental to III-V device performance. Details…

  • Purchase this item

    Indium Bar 6n5 WCI 500gIndium Bar 6n5 WCI 500g

    IPN: Ingoti6-05989-500gIG

    Price: $2.42

    "Our 6N5WCI (with controlled impurities) indium is refined for use in critical bulk crystal growth and in epitazial processes including molecular beam (MBE), liquid phase (LPE), and vapor phase (VPE) epitazy 6N5WCI is tailored for applications requiring the stringent control of impurities which, until now, only a 7N purity level may have provided at higher cost. This is accomplished by holding total metallic impurities to less than 500 ppb/weight (by GDMS), with particular attention given to maintaining low levels of elements known to be detrimental to III-V device performance." Details…

  • Purchase this item

    Sn62.5/Pb36/Ag1.5 Wave Solder BarSn62.5/Pb36/Ag1.5 Wave Solder Bar

    IPN: Ingotot-05104-500gIG

    Price: $250.00

    Indium Corporation of America's bar solder is a high purity material manufactured to provide consistent and reliable performance. Details…

  • Purchase this item

    Sn63/Pb37 Wave Solder BarSn63/Pb37 Wave Solder Bar

    IPN: Ingotot-05106-500gIG

    Price: $250.00

    Indium Corporation of America's bar solder is a high purity material manufactured to provide consistent and reliable performance. Details…