Bars:
Fusible Alloys, High Purity Indium Bars, Indium Alloy Bars, Pure Indium Bars, Pure Metal Bars (Non Indium), Wave Solder Bars
-
1lb 90In 10Sn Alloy BarIPN: Ingotia-05538-1lbIG
Price: $489.09
Indium-tin alloys are useful where lower temperatures are required to protect heat-sensitive components and substrates. The indium-tin eutectic with a sharp melting point has excellent wettability on nonmetallic materials. It also has good low-temperature malleability and compensates for some difference in the coefficients of thermal expansion of dissimilar metals. The addition of either metal to the other increases the corrosion resistance of the resulting alloy.
If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details… -
1lb 91In 9Sn Alloy BarIPN: Ingotia-05887-1lbIG
Price: $360.23
Indium-tin alloys are useful where lower temperatures are required to protect heat-sensitive components and substrates. The indium-tin eutectic with a sharp melting point has excellent wettability on nonmetallic materials. It also has good low-temperature malleability and compensates for some difference in the coefficients of thermal expansion of dissimilar metals. The addition of either metal to the other increases the corrosion resistance of the resulting alloy.
If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details… -
500g 99.9% In IngotIPN: Ingotic-05376-500gIG
Price: $0.87
Typical Indium Analysis
99.9%
PPMWT
Fe : 10-20
Ni : 5-20
Cu : 5-30
Cd : 50-100
Pb : 200-300
Sn : 50-200
Ti : 100-300
Analysis by OES
* Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.
If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details… -
500g 99.99% In IngotIPN: Ingotic-05373-500gIG
Price: $0.88
Typical Analysis
99.99% Indium
PPMWT
Fe : 1-2
Ni : 2-6
Cu : 2-6
Cd : 5-10
Pb : 10-30
Sn : 10-25
Ti : 1-4
Analysis by OES
* Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.
If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details… -
500g 99.999% In IngotIPN: Ingoti5-05374-500gIG
Price: $0.92
Typical Indium Analysis
99.999%
PPMWT
Fe : 0.5
Ni : 1.0
Cu : 1.0
Cd : 1.0
Pb : 2.0
Sn : 2.5
Ti : 1.0
Analysis by OES
* Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.
If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements. Details… -
Indium Bar 6n min 1kgIPN: Ingoti6-05375-1kIG
Price: $1310.00
We produce 6N material with impurities held to less than 100 ppb/weight as analyzed by OES. 6N (and often 5N) indium is selected when the user's application offers enough flexibility to allow the balancing of device performance with material cost. Details…