    Indium Acetate - Anhydrous PowderIndium Acetate - Anhydrous Powder

    IPN: saltah-71001-1kCON

    Price: $768.60

    General Description: White powder with chraracteristic acetic odor having a needle like crystalline morphology
    • Molecular Weight: 291.86
    • Theoretical Indium Content: 39.33%
    • Actual Indium Content Range: 40%-45%
    • Tap Density: <1
    • Purity: 99.99% minimum
    • Solubility: Freely soluble in mineral acids and acetic acid, slightly soluble in water Details…

  • Purchase this item

    Indium Hydroxide - Crystalline PowderIndium Hydroxide - Crystalline Powder

    IPN: saltah-71002-1kCON

    Price: $688.74

    Product Characteristics
    • Color: White
    • Molecular Weight: 165.84
    • %of Indium (Fine): 64-67%
    • % of Indium (Crystalline): 69.26%
    • Apparent Density: 1.2 gr/cc
    • Nominal d50 particle size: 20 microns
    • Safety Data: Available on request and shipped with product. Details…

  • Purchase this item

    Indium Hydroxide - Hydrated  PowderIndium Hydroxide - Hydrated Powder

    IPN: saltah-71140-1kCON

    Price: $425.70

    Product Characteristics
    • Color: White
    • Molecular Weight: 165.84
    • % of Indium (Fine): 64-67%
    • % of Indium (Crystalline): 69.26%
    • Apparent Density: 1.8gr/cc
    • Nominal d50 particle size: 2 microns
    • Safety Data: Available on request and shipped with product. Details…

  • Purchase this item

    Indium Nitrate - Anhydrous PowderIndium Nitrate - Anhydrous Powder

    IPN: saltah-71029-1kCON

    Price: $487.51

    General Information
    • Molecular Weight: 300.85 Anhydrous, 354.88 Hydrated
    • % of Indium: 38.16% (Anhydrous)
    • Specific Gravity: N/A
    • Melting Point: -2 H2O @ 100 Degrees C
    • Boiling Point: Decomposes
    • Solubility in Water: Very Soluble in water; soluble in alcohol
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Nitrate - Hydrated PowderIndium Nitrate - Hydrated Powder

    IPN: saltah-71014-1kCON

    Price: $432.29

    General Information
    • Molecular Weight: 300.86 Anhydrous, 354.88 Hydrated
    • % of Indium: 38.16% (Anhydrous)
    • Specific Gravity: N/A
    • Melting Point: -2 H2O @ 100 Degrees C
    • Boiling Point: Decomposes
    • Solubility in Water: Very Soluble in water; soluble in alcohol
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Oxide - Fine PowderIndium Oxide - Fine Powder

    IPN: saltah-71139-1kCON

    Price: $796.44

    Product Characteristics
    Color: Yellow
    Molecular Weight: 277.64 (82.7% IN, 17.3% O)
    Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2 g/cc)
    Nominal Tap Density: 1 gr/cc
    Nominal d50 Particle Size: 2.5 microns
    BET: 13 - 18 m2/gr
    Safety Data: Available on request and shipped with product. Details…

  • Purchase this item

    Indium Oxide - Standard PowderIndium Oxide - Standard Powder

    IPN: saltah-71044-1kCON

    Price: $766.82

    Product Characteristics
    Color: Yellow
    Formula Weight: 277.64 (82.7% In, 17.3% O)
    Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2 g/cc)
    Nominal Tap Density: 1.4 gr/cc
    Nominal d50 Particle Size: 17 microns
    BET: 2-3 m2/gr
    Safety Data: Available on request and shipped with product. Details…

  • Purchase this item

    Indium Sulfamate Plating BathIndium Sulfamate Plating Bath

    IPN: saltsl-72001-1glCON

    Price: $700.42

    Advantages of the Indium Sulfamate Bath
    • One of the easiest plating baths to operate and maintain
    • Proven formulation, capable of heavy production
    • Extremely stable operation and long life
    • Constant plating rate
    • Operates at room temperature
    • Wide current density range of operation
    • High, constant cathode efficiency of 90%
    • easy reclaim of indium from rinse waters
    • No addition agents required
    • Bath supplied ready to use
    • Indium replenishment is from indium anodes, not expensive bath concentrate requirements Details…

  • Purchase this item

    Indium Sulfate - Anhydrous PowderIndium Sulfate - Anhydrous Powder

    IPN: saltah-71047-1kCON

    Price: $845.70

    General Information
    • Molecular Weight: 517.81
    • %of Indium: 44.36%
    • Specific Gravity: 3.438 gr/cc, Apparent density N.A. Crystalline Form: White gray powder, monoclinic prisms, hydroscopic
    • Specific Heat: 0.129 cal/gram Degrees C (0-100 Degrees C)
    • Specific Heat: 49.039 cals (2 In + 3H2SO4 = In2(SO4)3 + 3H2 (g)) : 72.78 cals (In2O3 + 3H2S04 (adqueous solution) = In2(SO4)3 + 3H2O)
    • Dissociation Pressure: 10mm Hg @ 645 Degrees C 900mm Hg @ 820 Degrees C
    • Solubility in Water: 53.92 gr/100 gr solution @ 20 Degrees C
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Sulfate SolutionIndium Sulfate Solution

    IPN: saltsl-71149-1ltCON

    Price: $469.37

    General Information
    • Molecular Weight: 517.81
    • % of Indium : 44.36%
    • Specific Gravity: 3.438 gr/cc, Apparent density N.A.
    • Crystalline Form : white gray powder, monoclinic prisms, hydroscopic
    • Specific Heat : 0.129 cal/gram Degrees C (0-100 Degrees C) • Heat of Fromation : 49.039 cals (2 In + 3H2SO4 = In2(SO4)3 + 3H2 (g))
    • 72.78 cals (In2O3 + 3H2S04 (adqueous solution) = In2(SO4)3 + 3H2O)
    • Dissociation Pressure : 10mm Hg @ 645 Degrees C 900mm Hg @ 820 Degrees C
    • Solubility in Water : 53.92 gr/100 gr solution @ 20 Degrees C
    • Safety Data : Material Safety Data Sheet (MSDS) Available on request and shipped with product." Details…

  • Purchase this item

    Indium Sulfide - Anhydrous PowderIndium Sulfide - Anhydrous Powder

    IPN: saltah-71015-1kCON

    Price: $1033.25

    General Information
    • Molecular Weight: 325.82
    • % of Indium: 70.5%
    • Specific Gravity: 4.90 gr/cc, Apparent Density N/A
    • Melting Point: 1050 Degrees C
    • Boiling Point: Sublimes @ 850 Degrees C in high vacuum
    • Solubility in Water : Insoluble in cold water; soluble in acids, slightly soluble in Na2S
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Tin Oxide - Fine PowderIndium Tin Oxide - Fine Powder

    IPN: saltah-71159-1kCON

    Price: $759.96

    Product Characteristics
    • Color: Greenish Yellow
    • Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2g/cc)
    • Nominal Tap Density: 0.8 gr/cc
    • Nominal d50 particle size: 2 microns
    • BET: 15 m2/gr
    • Safety Data: Available on request and shipped with product. Details…

  • Purchase this item

    Indium Tin Oxide - Standard PowderIndium Tin Oxide - Standard Powder

    IPN: saltah-71099-1kCON

    Price: $751.96

    Product Characteristics
    • Color: Greenish Yellow
    • Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2g/cc)
    • Nominal Tap Density: 1.6 gr/cc
    • Nominal d50 Particle Size: 15 microns
    • BET: 2-3 m2/gr
    • Safety Data: Available on request and shipped with product. Details…

  • Purchase this item

    Indium Trichloride - Anhydrous PowderIndium Trichloride - Anhydrous Powder

    IPN: saltah-71008-1kCON

    Price: $762.83

    General Information
    • Molecular Weight: 221.18 Anhydrous (61.9 w/o In 48.1 w/o CI nominal value)
    • % of Indium : InCl3XH2o - 48%, INCl34H2O - 39%
    Specific Gravity: Solid 3.438 gr/cc, Apparent density N.A, SATURATED SOLUTION - 1.97
    • Melting Point: 586 Degrees C, sublimes @300 Degrees C
    • Boiling Point: Volitizes @ 600 Degrees C
    Solubility in Water: 66.11 grams/100grams of solution @ 22 Degrees C
    • Crystalline Form: White plates, deliquescent
    • Isomorphous: AlCl3, YCl3
    Coordination Number : 6
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Trichloride - Hydrated PowderIndium Trichloride - Hydrated Powder

    IPN: saltah-71070-1kCON

    Price: $702.12

    General Information
    • Molecular Weight: 221.18 Anhydrous (61.9 w/o In 48.1 w/o CI nominal value)
    • % of Indium: InCl3XH2o - 48%, INCl34H2O - 39%
    • Specific Gravity: Solid 3.438 gr/cc, Apparent density N.A, SATURATED SOLUTION - 1.97
    • Melting Point: 586 Degrees C, sublimes @300 Degrees C
    • Boiling Point: Volitizes @ 600 Degrees C
    • Solubility in Water: 66.11 grams/100grams of solution @ 22 Degrees C
    • Crystalline Form: White plates, deliquescent
    • Isomorphous: AlCl3, YCl3
    Coordination Number : 6
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Trichloride SolutionIndium Trichloride Solution

    IPN: saltsl-71154-1ltCON

    Price: $293.60

    General Information
    • Molecular Weight: 221.18 Anhydrous (61.9 w/o In 48.1 w/o CI nominal value)
    • % of Indium: InCl3XH2o - 48%, INCl34H2O - 39%
    • Specific Gravity: Solid 3.438 gr/cc, Apparent density N.A, SATURATED SOLUTION - 1.97
    • Melting Point: 586 Degrees C, sublimes @300 Degrees C
    • Boiling Point: Volitizes @ 600 Degrees C
    • Solubility in Water: 66.11 grams/100grams of solution @ 22 Degrees C
    • Crystalline Form: White plates, deliquescent
    • Isomorphous: AlCl3, YCl3
    Coordination Number: 6
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product." Details…

Shopping Cart:

Your cart is empty.

Search for