Chemicals:
Indium Chemical Powders, Indium Chemical Solutions
-
Indium Acetate - Anhydrous PowderIPN: saltah-71001-1kCON
Price: $823.85
General Description: White powder with chraracteristic acetic odor having a needle like crystalline morphology
• Molecular Weight: 291.86
• Theoretical Indium Content: 39.33%
• Actual Indium Content Range: 40%-45%
• Tap Density: <1
• Purity: 99.99% minimum
• Solubility: Freely soluble in mineral acids and acetic acid, slightly soluble in water Details… -
Indium Hydroxide - Crystalline PowderIPN: saltah-71002-1kCON
Price: $778.78
Product Characteristics
• Color: White
• Molecular Weight: 165.84
• %of Indium (Fine): 64-67%
• % of Indium (Crystalline): 69.26%
• Apparent Density: 1.2 gr/cc
• Nominal d50 particle size: 20 microns
• Safety Data: Available on request and shipped with product. Details… -
Indium Hydroxide - Hydrated PowderIPN: saltah-71140-1kCON
Price: $511.50
Product Characteristics
• Color: White
• Molecular Weight: 165.84
• % of Indium (Fine): 64-67%
• % of Indium (Crystalline): 69.26%
• Apparent Density: 1.8gr/cc
• Nominal d50 particle size: 2 microns
• Safety Data: Available on request and shipped with product. Details… -
Indium Nitrate - Anhydrous PowderIPN: saltah-71029-1kCON
Price: $538.12
General Information
• Molecular Weight: 300.85 Anhydrous, 354.88 Hydrated
• % of Indium: 38.16% (Anhydrous)
• Specific Gravity: N/A
• Melting Point: -2 H2O @ 100 Degrees C
• Boiling Point: Decomposes
• Solubility in Water: Very Soluble in water; soluble in alcohol
• Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details… -
Indium Nitrate - Hydrated PowderIPN: saltah-71014-1kCON
Price: $474.48
General Information
• Molecular Weight: 300.86 Anhydrous, 354.88 Hydrated
• % of Indium: 38.16% (Anhydrous)
• Specific Gravity: N/A
• Melting Point: -2 H2O @ 100 Degrees C
• Boiling Point: Decomposes
• Solubility in Water: Very Soluble in water; soluble in alcohol
• Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details… -
Indium Oxide - Fine PowderIPN: saltah-71139-1kCON
Price: $903.95
Product Characteristics
Color: Yellow
Molecular Weight: 277.64 (82.7% IN, 17.3% O)
Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2 g/cc)
Nominal Tap Density: 1 gr/cc
Nominal d50 Particle Size: 2.5 microns
BET: 13 - 18 m2/gr
Safety Data: Available on request and shipped with product. Details…