    Indium Oxide - Standard PowderIndium Oxide - Standard Powder

    IPN: saltah-71044-1kCON

    Price: $799.90

    Product Characteristics
    Color: Yellow
    Formula Weight: 277.64 (82.7% In, 17.3% O)
    Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2 g/cc)
    Nominal Tap Density: 1.4 gr/cc
    Nominal d50 Particle Size: 17 microns
    BET: 2-3 m2/gr
    Safety Data: Available on request and shipped with product. Details…

  • Purchase this item

    Indium Sulfamate Plating BathIndium Sulfamate Plating Bath

    IPN: saltsl-72001-1glCON

    Price: $705.02

    Advantages of the Indium Sulfamate Bath
    • One of the easiest plating baths to operate and maintain
    • Proven formulation, capable of heavy production
    • Extremely stable operation and long life
    • Constant plating rate
    • Operates at room temperature
    • Wide current density range of operation
    • High, constant cathode efficiency of 90%
    • easy reclaim of indium from rinse waters
    • No addition agents required
    • Bath supplied ready to use
    • Indium replenishment is from indium anodes, not expensive bath concentrate requirements Details…

  • Purchase this item

    Indium Sulfate - Anhydrous PowderIndium Sulfate - Anhydrous Powder

    IPN: saltah-71047-1kCON

    Price: $862.90

    General Information
    • Molecular Weight: 517.81
    • %of Indium: 44.36%
    • Specific Gravity: 3.438 gr/cc, Apparent density N.A. Crystalline Form: White gray powder, monoclinic prisms, hydroscopic
    • Specific Heat: 0.129 cal/gram Degrees C (0-100 Degrees C)
    • Specific Heat: 49.039 cals (2 In + 3H2SO4 = In2(SO4)3 + 3H2 (g)) : 72.78 cals (In2O3 + 3H2S04 (adqueous solution) = In2(SO4)3 + 3H2O)
    • Dissociation Pressure: 10mm Hg @ 645 Degrees C 900mm Hg @ 820 Degrees C
    • Solubility in Water: 53.92 gr/100 gr solution @ 20 Degrees C
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Sulfate SolutionIndium Sulfate Solution

    IPN: saltsl-71149-1ltCON

    Price: $474.37

    General Information
    • Molecular Weight: 517.81
    • % of Indium : 44.36%
    • Specific Gravity: 3.438 gr/cc, Apparent density N.A.
    • Crystalline Form : white gray powder, monoclinic prisms, hydroscopic
    • Specific Heat : 0.129 cal/gram Degrees C (0-100 Degrees C) • Heat of Fromation : 49.039 cals (2 In + 3H2SO4 = In2(SO4)3 + 3H2 (g))
    • 72.78 cals (In2O3 + 3H2S04 (adqueous solution) = In2(SO4)3 + 3H2O)
    • Dissociation Pressure : 10mm Hg @ 645 Degrees C 900mm Hg @ 820 Degrees C
    • Solubility in Water : 53.92 gr/100 gr solution @ 20 Degrees C
    • Safety Data : Material Safety Data Sheet (MSDS) Available on request and shipped with product." Details…

  • Purchase this item

    Indium Sulfide - Anhydrous PowderIndium Sulfide - Anhydrous Powder

    IPN: saltah-71015-1kCON

    Price: $1061.45

    General Information
    • Molecular Weight: 325.82
    • % of Indium: 70.5%
    • Specific Gravity: 4.90 gr/cc, Apparent Density N/A
    • Melting Point: 1050 Degrees C
    • Boiling Point: Sublimes @ 850 Degrees C in high vacuum
    • Solubility in Water : Insoluble in cold water; soluble in acids, slightly soluble in Na2S
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Tin Oxide - Fine PowderIndium Tin Oxide - Fine Powder

    IPN: saltah-71159-1kCON

    Price: $789.73

    Product Characteristics
    • Color: Greenish Yellow
    • Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2g/cc)
    • Nominal Tap Density: 0.8 gr/cc
    • Nominal d50 particle size: 2 microns
    • BET: 15 m2/gr
    • Safety Data: Available on request and shipped with product. Details…