    Indium Tin Oxide - Standard PowderIndium Tin Oxide - Standard Powder

    IPN: saltah-71099-1kCON

    Price: $781.73

    Product Characteristics
    • Color: Greenish Yellow
    • Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2g/cc)
    • Nominal Tap Density: 1.6 gr/cc
    • Nominal d50 Particle Size: 15 microns
    • BET: 2-3 m2/gr
    • Safety Data: Available on request and shipped with product. Details…

  • Purchase this item

    Indium Trichloride - Anhydrous PowderIndium Trichloride - Anhydrous Powder

    IPN: saltah-71008-1kCON

    Price: $783.59

    General Information
    • Molecular Weight: 221.18 Anhydrous (61.9 w/o In 48.1 w/o CI nominal value)
    • % of Indium : InCl3XH2o - 48%, INCl34H2O - 39%
    Specific Gravity: Solid 3.438 gr/cc, Apparent density N.A, SATURATED SOLUTION - 1.97
    • Melting Point: 586 Degrees C, sublimes @300 Degrees C
    • Boiling Point: Volitizes @ 600 Degrees C
    Solubility in Water: 66.11 grams/100grams of solution @ 22 Degrees C
    • Crystalline Form: White plates, deliquescent
    • Isomorphous: AlCl3, YCl3
    Coordination Number : 6
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Trichloride - Hydrated PowderIndium Trichloride - Hydrated Powder

    IPN: saltah-71070-1kCON

    Price: $718.81

    General Information
    • Molecular Weight: 221.18 Anhydrous (61.9 w/o In 48.1 w/o CI nominal value)
    • % of Indium: InCl3XH2o - 48%, INCl34H2O - 39%
    • Specific Gravity: Solid 3.438 gr/cc, Apparent density N.A, SATURATED SOLUTION - 1.97
    • Melting Point: 586 Degrees C, sublimes @300 Degrees C
    • Boiling Point: Volitizes @ 600 Degrees C
    • Solubility in Water: 66.11 grams/100grams of solution @ 22 Degrees C
    • Crystalline Form: White plates, deliquescent
    • Isomorphous: AlCl3, YCl3
    Coordination Number : 6
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product. Details…

  • Purchase this item

    Indium Trichloride SolutionIndium Trichloride Solution

    IPN: saltsl-71154-1ltCON

    Price: $295.67

    General Information
    • Molecular Weight: 221.18 Anhydrous (61.9 w/o In 48.1 w/o CI nominal value)
    • % of Indium: InCl3XH2o - 48%, INCl34H2O - 39%
    • Specific Gravity: Solid 3.438 gr/cc, Apparent density N.A, SATURATED SOLUTION - 1.97
    • Melting Point: 586 Degrees C, sublimes @300 Degrees C
    • Boiling Point: Volitizes @ 600 Degrees C
    • Solubility in Water: 66.11 grams/100grams of solution @ 22 Degrees C
    • Crystalline Form: White plates, deliquescent
    • Isomorphous: AlCl3, YCl3
    Coordination Number: 6
    • Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product." Details…