Shot

Shot:

Shot are tear-dropped shaped pieces of metal that are typically used to weigh quantities of other alloys. Examples include: filling vapor deposition crucibles or filling anode baskets with indium for electroplating.

  • Purchase this item

    High Purity Indium ShotHigh Purity Indium Shot

    IPN: Shoti6-47506-1kgGJ

    Price: $1435.00

    We produce 6N material with impurities held to less than 100 ppb/weight as analyzed by OES. 6N (and often 5N) indium is selected when the user's application offers enough flexibility to allow the balancing of device performance with material cost.

    Size: .125" Diameter approx; Random Sized Teardrop Shaped Details…

  • Purchase this item

    High Purity Indium ShotHigh Purity Indium Shot

    IPN: Shoti6-47562-1kgGJ

    Price: $1535.00

    This purity is especially suited for the production of single crystal III-V compound semiconductors, such as Indium Phosphide used as substrates for fabrication of integrated circuits or discrete devices such as laser diodes and photo detectors, Certification of 6N5 purity is by OES (optical emission spectoscopy) with GFAA (graphite furnace atomic absorption) being used for quantitative analysis of selected elements.

    Size: .125" Diameter approx; Random Sized Teardrop Shaped Details…

  • Purchase this item

    High Purity Indium ShotHigh Purity Indium Shot

    IPN: Shoti6-47567-1kgGJ

    Price: $1985.00

    Our 6N5WCI (with controlled impurities) indium is refined for use in critical bulk crystal growth and in epitazial processes including molecular beam (MBE), liquid phase (LPE), and vapor phase (VPE) epitazy 6N5WCI is tailored for applications requiring the stringent control of impurities which, until now, only a 7N purity level may have provided at higher cost. This is accomplished by holding total metallic impurities to less than 500 ppb/weight (by GDMS), with particular attention given to maintaining low levels of elements known to be detrimental to III-V device performance.

    Size: .125" Diameter approx; Random Sized Teardrop Shaped Details…

  • Purchase this item

    Pure Indium ShotPure Indium Shot

    IPN: Shoti5-47505-1kGJ

    Price: $960.00

    Typical Indium Analysis
    99.999%


    PPMWT
    Fe : 0.5
    Ni : 1.0
    Cu : 1.0
    Cd : 1.0
    Pb : 2.0
    Sn : 2.5
    Ti : 1.0

    Analysis by OES

    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements.

    Size: .125" diameter, Random sized; Teardrop Shaped Details…

  • Purchase this item

    Pure Indium ShotPure Indium Shot

    IPN: Shotic-47504-1kPJ

    Price: $920.00

    Typical Indium Analysis
    99.99%


    PPMWT
    Fe : 1-2
    Ni : 2-6
    Cu : 2-6
    Cd : 5-10
    Pb : 10-30
    Sn : 10-25
    Ti : 1-4

    Analysis by OES

    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements.

    Size: .125" diameter, Random sized; Teardrop Shaped Details…

  • Purchase this item

    Pure Indium ShotPure Indium Shot

    IPN: Shotic-47507-1kPJ

    Price: $902.50

    Typical Indium Analysis
    99.9%


    PPMWT
    Fe : 10-20
    Ni : 5-20
    Cu : 5-30
    Cd : 50-100
    Pb : 200-300
    Sn : 50-200
    Ti : 100-300

    Analysis by OES

    * Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

    If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements.

    Size: .125" diameter, Random sized; Teardrop Shaped Details…

Shopping Cart:

Your cart is empty.

Search for