    This solid core solder wire is three feet long and is packaged in a tube. The diameter is .030".

    Composition: 62n 36Pb 2Ag
    Diameter: .030"
    Packaging: 3 ft. Spool
    Unit of Measure: Spool Details…

  • Purchase this item

    WireWire

    IPN: Wirein-51999-3ftSP

    Price: $350.00

    This solid core solder wire is three feet long and is packaged in a tube. The diameter is .030".

    Composition: 99.99ln
    Diameter: .030"
    Packaging: 3 ft Spool
    Unit of Measure: Spool Details…

  • Purchase this item

    WireWire

    IPN: Wireot-51237-3ftSP

    Price: $180.00

    This solid core solder wire is three feet long and is packaged in a tube. The diameter is .030".

    Composition: 46Bi 34Sn 20Pb
    Diameter: .030"
    Packaging: 3 ft Spool
    Unit of Measure: Spool Details…

  • Purchase this item

    WireWire

    IPN: Wirein-50613-3ftSP

    Price: $350.00

    This solid core solder wire is three feet long and is packaged in a tube. The diameter is .030".

    Composition: 49Bi 21ln 18Pb 12Sn
    Diameter: .030"
    Packaging: 3 ft Spool
    Unit of Measure: Spool Details…

  • Purchase this item

    WireWire

    IPN: Wirein-51168-3ftSP

    Price: $350.00

    This solid core solder wire is three feet long and is packaged in a tube. The diameter is .030".

    Composition: 52ln 48Sn
    Diameter: .030"
    Packaging: 3 ft Spool
    Unit of Measure: Spool Details…

  • Purchase this item

    WireWire

    IPN: Wireot-51035-3ftSP

    Price: $180.00

    This solid core solder wire is three feet long and is packaged in a tube. The diameter is .030".

    Composition: 58Bi 42Sn
    Diameter: .030"
    Packaging: 3 ft Spool
    Unit of Measure: Spool Details…