1kg 99.9% In Ingot
IPN: Ingotic-05376-1kIG
Price: $802.50
| price per item | minimum qty. |
|---|---|
| $ 802.50 | 1+ |
| $ 774.00 | 2+ |
| $ 603.00 | 5+ |
| $ 536.50 | 10+ |
| $ 508.00 | 15+ |
Product Description:
Typical Indium Analysis
99.9%
PPMWT
Fe : 10-20
Ni : 5-20
Cu : 5-30
Cd : 50-100
Pb : 200-300
Sn : 50-200
Ti : 100-300
Analysis by OES
* Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.
If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements.