High Purity Indium Shot
IPN: Shoti6-47506-1kgGJ
Price: $1345.00
| price per item | minimum qty. |
|---|---|
| $ 1345.00 | 1+ |
| $ 995.00 | 3+ |
| $ 815.00 | 5+ |
| $ 755.00 | 10+ |
Product Description:
We produce 6N material with impurities held to less than 100 ppb/weight as analyzed by OES. 6N (and often 5N) indium is selected when the user's application offers enough flexibility to allow the balancing of device performance with material cost.
Size: .125" Diameter approx; Random Sized Teardrop Shaped