Indium Bar 6n min 1kg
IPN: Ingoti6-05375-1kIG
Price: $1270.00
| price per item | minimum qty. |
|---|---|
| $ 1270.00 | 1+ |
| $ 920.00 | 3+ |
| $ 740.00 | 5+ |
| $ 680.00 | 10+ |
Product Description:
We produce 6N material with impurities held to less than 100 ppb/weight as analyzed by OES. 6N (and often 5N) indium is selected when the user's application offers enough flexibility to allow the balancing of device performance with material cost.