Indium Bar 6n min 500g

IPN: Ingoti6-05375-500gIG

Price: $1.88

Indium Bar 6n min 500g
Purchase this item
Quantity Discounts
price per itemminimum qty.
$ 1.88 500+
$ 1.27 1000+
$ 0.93 3000+
$ 0.74 5000+
$ 0.69 10000+

Product Description:

We produce 6N material with impurities held to less than 100 ppb/weight as analyzed by OES. 6N (and often 5N) indium is selected when the user's application offers enough flexibility to allow the balancing of device performance with material cost.