Indium Bar 6n5 WCI 1kg

IPN: Ingoti6-05989-1kIG

Price: $1820.00

Indium Bar 6n5 WCI 1kg
Purchase this item
Quantity Discounts
price per itemminimum qty.
$ 1820.00 1+
$ 1360.00 3+
$ 1180.00 5+
$ 1040.00 10+

Product Description:

Our 6N5WCI (with controlled impurities) indium is refined for use in critical bulk crystal growth and in epitazial processes including molecular beam (MBE), liquid phase (LPE), and vapor phase (VPE) epitazy 6N5WCI is tailored for applications requiring the stringent control of impurities which, until now, only a 7N purity level may have provided at higher cost. This is accomplished by holding total metallic impurities to less than 500 ppb/weight (by GDMS), with particular attention given to maintaining low levels of elements known to be detrimental to III-V device performance.