Product Description:
Product Characteristics
• Color: White
• Molecular Weight: 165.84
• %of Indium (Fine): 64-67%
• % of Indium (Crystalline): 69.26%
• Apparent Density: 1.2 gr/cc
• Nominal d50 particle size: 20 microns
• Safety Data: Available on request and shipped with product.