Indium Oxide - Standard Powder

IPN: saltah-71044-1kCON

Price: $766.82

Indium Oxide - Standard Powder
Purchase this item
Quantity Discounts
price per itemminimum qty.
$ 766.82 1+
$ 615.66 2+
$ 550.23 5+
$ 484.82 10+
$ 469.39 20+
$ 453.97 35+

Product Description:

Product Characteristics
Color: Yellow
Formula Weight: 277.64 (82.7% In, 17.3% O)
Specific Gravity: 7.2 g/cc (Apparent Density 0.5-1.2 g/cc)
Nominal Tap Density: 1.4 gr/cc
Nominal d50 Particle Size: 17 microns
BET: 2-3 m2/gr
Safety Data: Available on request and shipped with product.