Product Description:
General Information
• Molecular Weight: 517.81
• %of Indium: 44.36%
• Specific Gravity: 3.438 gr/cc, Apparent density N.A. Crystalline Form: White gray powder, monoclinic prisms, hydroscopic
• Specific Heat: 0.129 cal/gram Degrees C (0-100 Degrees C)
• Specific Heat: 49.039 cals (2 In + 3H2SO4 = In2(SO4)3 + 3H2 (g)) : 72.78 cals (In2O3 + 3H2S04 (adqueous solution) = In2(SO4)3 + 3H2O)
• Dissociation Pressure: 10mm Hg @ 645 Degrees C 900mm Hg @ 820 Degrees C
• Solubility in Water: 53.92 gr/100 gr solution @ 20 Degrees C
• Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product.