Indium Sulfate Solution

IPN: saltsl-71149-1ltCON

Price: $469.37

Indium Sulfate Solution
Purchase this item
Quantity Discounts
price per itemminimum qty.
$ 469.37 1+
$ 314.55 2+
$ 284.22 8+
$ 253.89 20+

Product Description:

General Information
• Molecular Weight: 517.81
• % of Indium : 44.36%
• Specific Gravity: 3.438 gr/cc, Apparent density N.A.
• Crystalline Form : white gray powder, monoclinic prisms, hydroscopic
• Specific Heat : 0.129 cal/gram Degrees C (0-100 Degrees C) • Heat of Fromation : 49.039 cals (2 In + 3H2SO4 = In2(SO4)3 + 3H2 (g))
• 72.78 cals (In2O3 + 3H2S04 (adqueous solution) = In2(SO4)3 + 3H2O)
• Dissociation Pressure : 10mm Hg @ 645 Degrees C 900mm Hg @ 820 Degrees C
• Solubility in Water : 53.92 gr/100 gr solution @ 20 Degrees C
• Safety Data : Material Safety Data Sheet (MSDS) Available on request and shipped with product."