Indium Sulfide - Anhydrous Powder

IPN: saltah-71015-1kCON

Price: $1033.25

Indium Sulfide - Anhydrous Powder
Purchase this item
Quantity Discounts
price per itemminimum qty.
$ 1033.25 1+
$ 884.59 2+
$ 758.84 5+
$ 733.08 10+
$ 707.33 20+
$ 681.57 35+

Product Description:

General Information
• Molecular Weight: 325.82
• % of Indium: 70.5%
• Specific Gravity: 4.90 gr/cc, Apparent Density N/A
• Melting Point: 1050 Degrees C
• Boiling Point: Sublimes @ 850 Degrees C in high vacuum
• Solubility in Water : Insoluble in cold water; soluble in acids, slightly soluble in Na2S
• Safety Data: Material Safety Data Sheet (MSDS) Available on request and shipped with product.