General Information
• Molecular Weight: 221.18 Anhydrous (61.9 w/o In 48.1 w/o CI nominal value)
• % of Indium: InCl3XH2o - 48%, INCl34H2O - 39%
• Specific Gravity: Solid 3.438 gr/cc, Apparent density N.A, SATURATED SOLUTION - 1.97
• Melting Point: 586 Degrees C, sublimes @300 Degrees C
• Boiling Point: Volitizes @ 600 Degrees C
• Solubility in Water: 66.11 grams/100grams of solution @ 22 Degrees C
• Crystalline Form: White plates, deliquescent
• Isomorphous: AlCl3, YCl3
Coordination Number: 6