Pure Indium Shot

IPN: Shoti5-47505-1kGJ

Price: $880.00

Pure Indium Shot
Purchase this item
Quantity Discounts
price per itemminimum qty.
$ 880.00 1+
$ 847.00 2+
$ 649.00 5+
$ 572.00 10+
$ 539.00 15+

Product Description:

Typical Indium Analysis
99.999%


PPMWT
Fe : 0.5
Ni : 1.0
Cu : 1.0
Cd : 1.0
Pb : 2.0
Sn : 2.5
Ti : 1.0

Analysis by OES

* Please note that these are typical ppm levels, and do not represent maximum, minimum, or lot specific levels.

If you have specific requirements for one or two elements, we would be pleased to review our ability to accommodate those requirements. Please submit a request for quotation, outlining your specific requirements.

Size: .125" diameter, Random sized; Teardrop Shaped