Wire
IPN: Wirein-50613-3ftSP
Price: $350.00
Product Description:
This solid core solder wire is three feet long and is packaged in a tube. The diameter is .030".
Composition: 49Bi 21ln 18Pb 12Sn
Diameter: .030"
Packaging: 3 ft Spool